Why is joining composite parts an engineering subject?
Most structures cannot be made in one piece, or it is not economical to do so; platforms, handrails, stairs, cable tray supports and covers are built from separate profiles and parts joined on site. Unlike steel, thermoset composite parts cannot be welded, because cured resin does not melt. For this reason, the methods of joining composite parts fall into three main groups:
- Mechanical joints: bolts and nuts, rivets, pins and self-tapping screws.
- Adhesive joints: joining two surfaces with a structural adhesive.
- Hybrid joints: using adhesive and mechanical fastening together.
Joints are critical in composites because their properties are anisotropic: a pultruded profile is very strong in the fiber (longitudinal) direction, but its transverse strength, interlaminar shear strength and bearing resistance are lower, and its behavior up to failure is almost linear with no yielding. So, unlike steel, stress at a joint is not redistributed between bolts by local yielding, and the joint geometry matters more. See the design principles in design and analysis of composites.
Mechanical versus adhesive joints in composites
The choice between a mechanical and an adhesive joint depends on part thickness, load type, environmental conditions, the need for disassembly and the workshop facilities. The table below compares the advantages and disadvantages of each method:
| Criterion | Mechanical joints (bolt, rivet, pin) | Adhesive joints |
|---|---|---|
| Thickness limit | None; suits thick parts | More efficient for thin to medium parts |
| Disassembly and inspection | Can be taken apart and inspected without damage | Permanent; inspection needs non-destructive methods |
| Preparation | Accurate drilling | Surface preparation, environmental control and cure time |
| Stress concentration | Severe concentration at the hole edge | Spread over the area; stress peaks at both ends of the overlap |
| Fiber cutting | The hole cuts the fibers | Fibers stay intact |
| Weight | Bolts and connection plates add weight | Lighter |
| Fatigue and sealing | Sensitive to slack and moisture ingress through the hole | Good fatigue performance and sealed |
| Sensitivity to environment and workmanship | Low; simple to do on site | High; sensitive to temperature, humidity and surface cleanliness |
| Residual stress and corrosion | Creates no residual stress | May arise from cure shrinkage and differential thermal expansion |
| Failure behavior | Gradual (especially in bearing) | Often sudden |
Mechanical joints in composite parts
Mechanical joints are the most common way of joining composite parts in pultruded structures, platforms and handrails. The types of mechanical joint are:
Drilling composite parts
Every mechanical joint starts with drilling, and the quality of the hole determines the quality of the joint. The greatest risk when drilling composites is delamination and fraying of the fibers on the entry side and especially the exit side of the drill. To prevent it:
- Use a sharp diamond or carbide drill; an ordinary HSS drill blunts quickly and tears the fibers.
- Keep the feed force on the drill low and steady, especially as the drill breaks through; place a backing board (wood or scrap composite) under the part.
- Choose a suitable cutting speed and a slow feed, and where possible use coolant (water) to reduce heat and dust.
- Choose a drill about 0.5 to 1 mm larger than the bolt diameter (a close-clearance hole). In structural joints where load sharing between bolts matters, less clearance is better.
- Seal the hole wall and cut edges with resin so that moisture cannot penetrate the cut fibers.
See tooling and speeds in cutting and machining composites.
Hole location: hole spacing and edge distance
The spacing between holes and the distance from a hole to the outer edge of the composite part determine the failure mode of the joint. Too small a spacing makes the stress concentrations around the holes overlap and causes premature failure of the joint in brittle modes (shear-out or cleavage).
In the table below, d is the hole diameter. To reach maximum bearing capacity and gradual failure, a larger end distance e (about 4 × d) is recommended.
Meeting these distances in narrow parts such as flat bars and channel flanges limits the number and diameter of bolts that can be used; in that case the usual solution is to use two smaller bolts instead of one large bolt, or to widen the connection plate.
| Parameter | Symbol | Minimum allowable distance |
|---|---|---|
| Hole center to end edge (in the load direction) | e | 2.5 × d |
| Hole center to side edge | c | 2.5 × d |
| Hole center-to-center spacing in the load direction | p₁ | 4 × d |
| Hole center-to-center spacing perpendicular to the load | p₂ | 4 × d |
Failure modes of bolted composite joints
A bolted composite joint can fail in one of the modes below. The aim of design is to make bearing the failure mode through correct spacing, because it is the only mode that develops gradually and gives warning (deformation and slack) before complete failure:
- Bearing: crushing of the composite in front of the bolt; the desirable mode. Its main drawback is increasing slack.
- Net-section tension: failure of the remaining section beside the hole; when the side distance c or the part width is small.
- Shear-out: a piece of the part in front of the bolt is pushed out along the fibers; when the end distance e is small. Very common in pultrusion because of the low shear strength.
- Cleavage: a combination of tension and shear — a longitudinal crack from the hole to the edge. Occurs with a small end distance and few transverse fibers.
Technical tips for a good mechanical joint
- Two wide flat washers: one under the bolt head and one under the nut, to spread the pressure evenly and prevent surface crushing. The outer diameter of the flat washer should be at least 3 times the hole diameter.
- Locking the nut: to prevent loosening under vibration, use a spring (lock) washer on top of a metal flat washer, or preferably a nylon-insert lock nut. A spring washer must never bear directly on the composite surface, because its sharp edge digs into the resin.
- Sleeves in hollow and thick sections: in box sections, tubes and thick parts, use a composite, plastic or metal sleeve (spacer) sized to the hole to increase resistance to tightening torque and prevent the walls from being crushed.
- Limited torque: the torque needed to tighten a bolt in a composite part is lower than in metal. Tighten bolts "firmly", not "as tight as possible"; use a torque wrench and the values recommended by the manufacturer. Excessive torque causes crushing, resin cracking and delamination at the joint.
- Bolt material: in corrosive environments, 316 (A4) stainless steel is the first choice; the cheaper 304 (A2) stainless steel can be used in milder environments or if 316 is not available. Galvanized steel in a corrosive environment will not last as long as the composite. For electrically insulating applications, use composite (FRP) bolts and nuts.
- Self-tapping screws: only for lightly loaded parts (covers, lids, light frames). First drill a pilot hole of about the thread root diameter (usually about 2 mm smaller than the nominal screw diameter), then install the self-tapping screw. Self-tapping screws have limited pull-out capacity in composites.
- Rivets: for thin parts such as sheets, ducts and covers; use stainless or aluminum rivets with backing washers, or large-flange rivets, so the composite does not crack.
- Pins: a steel or composite pin is inserted into a pre-drilled hole with adhesive; common in handrail and stair connections.
Practical details of mechanical joints in composite structures
In profile structures, column-to-base-plate, column-to-beam and beam-to-beam connections are made with composite or steel angles and connection plates and bolts. The examples below show common connection details for channel, box and I-section profiles (each figure shows the connection view and section A-A):
Joint selection table for composite profiles and parts
The table below summarizes the recommended method — mechanical, adhesive or hybrid — for the most common details in composite structures, from an I-section column to base plate through to sheet and pipe joints:
| Connection detail | Recommended method | Practical note |
|---|---|---|
| Channel to flat bar | Mechanical joints (bolts and nuts) | At least two bolts; wide washer on the flat bar |
| Channel column to floor base plate | Bolts and nuts with angles | Fiberglass or steel angle on both sides of the channel web |
| Box column to floor base plate | Through-bolt with sleeve | Sleeve inside the box section to prevent wall crushing |
| I-section column to floor base plate | Bolts and nuts with angles | Connect the web of the I-section column; flanges free |
| Box column to channel beam | Mechanical or hybrid joints | Through-bolt in the box section with sleeve; adhesive for extra stiffness |
| I-section column to channel beam | Bolts and nuts | The channel beam is bolted to the flange of the I-section column |
| I-section column to I-beam | Web and flange connection angles | Pinned connection; lateral bracing required |
| Two nested channel beams | Bolts and nuts | Sufficient overlap and hole spacing ≥ 4d |
| Horizontal connection of two I-beams | Angles and bolts | Cope the flange of the secondary beam and connect to the web of the main beam |
| Fiberglass sheet and covers | Rivets, self-tapping screws or adhesive joints | Wide sealing washer; pre-drilling |
| Fiberglass pipe | Adhesive joints (spigot and socket) or bolted flanges | Bonding with resin and surface preparation |
| Composite grating | M and C clips | No drilling of the panel |
In all these joints, following the drilling and spacing rules controls stress concentration. Unlike metals, corrosion of the composite itself is not an issue in composite parts; but corrosion of metal bolts and connection plates, and galvanic corrosion where carbon fiber touches aluminum or steel, must be controlled by choosing 316 stainless steel or insulating between the surfaces.
Adhesive joints in composite parts
In an adhesive joint, two surfaces are joined by a layer of structural adhesive. With a suitable bonding process, two composite parts, or a composite part and a metal part, can be bonded together. When bonding composite to metal, the difference in thermal expansion (especially with aluminum) means temperature changes create additional stress in the bond line, which must be controlled by choosing a more flexible adhesive and a suitable bond-line thickness. In addition, gaps and clearances in mechanical joints can be filled with a special adhesive so that load is shared better between the bolts.
Types of adhesive joint in composites
The three main types of adhesive joint (lap, stepped and scarf) are chosen according to part thickness and joint location. The quality of these adhesive joints depends more on bonding workmanship and surface preparation than on the type of adhesive.
- Single-lap joint: the simplest and most common; because the load path is eccentric, it has high peel stress at the edges.
- Double-lap joint and strap joint: eliminate secondary bending and roughly double the capacity.
- Stepped joint: thickness reduced in steps; suits thick parts.
- Scarf joint: the most efficient adhesive joint, with almost uniform stress distribution; widely used in repairing composite parts, but requires precise machining.
Steps in bonding composite parts
- Surface preparation: sanding (about P80 to P120) to remove the glossy resin layer and mold release, or removing the peel ply just before bonding.
- Cleaning: removing dust and wiping with a suitable solvent (acetone or isopropyl alcohol), then waiting for it to evaporate completely.
- Applying the adhesive: epoxy, methacrylate (MMA) or polyurethane structural adhesives at the exact mix ratio; bond-line thickness usually 0.2 to 1 mm (per the adhesive datasheet).
- Assembly and fixing: placing the parts within the adhesive's working time and holding them with clamps or temporary bolts without excessive pressure.
- Curing: observe the cure time and temperature before loading; low ambient temperature lengthens the cure time.
See the standard adhesive joint tests (ASTM D5868 and ASTM D3163) in the composite testing standards article. Choosing a compatible resin and adhesive is also explained in types of composite resin.
Hybrid mechanical and adhesive joints
One of the most reliable ways of joining composite parts is to use adhesive and bolts together. In these hybrid joints, the adhesive, being stiffer, carries most of the service load with an even distribution over the area, fills the hole clearances and seals the joint; the bolts act as clamps while the adhesive cures and, if the adhesive is damaged or ages, act as a "fail-safe" backup load path that prevents sudden failure of the joint. The result is a relatively monolithic joint, higher fatigue resistance and safer failure behavior.
Welding composites: only for thermoplastics
Thermoset composite parts cannot be welded; but thermoplastic-matrix composites (such as fiber-reinforced polypropylene and polyamide) can be joined by ultrasonic welding, induction welding, resistance welding or hot plate welding. These methods are growing in the automotive and aerospace industries but are not common in pultruded products and grating.
Joining and installing Nabak composite products
Nabak profiles — composite channels, composite I-beams, box sections and composite flat bars — are compatible with all the mechanical and adhesive joints in this article; corrugated fiberglass and flat sheets are installed with rivets or self-tapping screws, fiberglass pipe with adhesive and flanged joints, and composite rods and polymer bars with pins and adhesive. Mechanical and adhesive joints are used to install all kinds of composite products, including fiberglass sheet (corrugated fiberglass), composite grating, composite box sections, fiberglass angles, composite channels, composite beams, fiberglass pipe, composite flat bars, polymer rods, composite wire and cable trays and ladders. For grating, special clips (M and C type) fix the grating to the substructure beam without drilling the panel; see the details in the grating selection guide.
Checklist for joining composite parts
This checklist turns the joining methods described into practical steps in the workshop and on site:
- Choose the method: thick part or need for disassembly → mechanical joint; thin part or sealing → adhesive joint; critical joint or vibration → hybrid joint.
- Check the geometry: hole-to-edge distance at least 2.5d and hole spacing at least 4d.
- Drill correctly: diamond drill, low pressure, backing board, drill 0.5 to 1 mm larger than the bolt.
- Seal: seal the hole wall and cut edges with resin.
- Complete the fixings: two wide flat washers, lock nut, sleeve in hollow sections.
- Limit the torque: torque wrench and the manufacturer's values; no surface crushing.
- Control adhesive joints: bond only to sanded, clean surfaces; record cure temperature and time.
- Inspect: after a few weeks in service, inspect the bolts and retighten if necessary.
Frequently asked questions about joining composite parts
Can composite parts be welded?
Thermoset composite parts such as polyester and vinyl ester profiles and grating cannot be welded, because cured resin does not melt. They are joined with bolts and nuts, rivets, pins, adhesive or a combination of adhesive and bolts. Only thermoplastic composites can be welded, with methods such as induction or ultrasonic welding.
What is the minimum distance from a bolt hole to the edge of a composite profile?
As a general rule, the distance from the hole center to the end edge and the side edge is taken as at least 2.5 times the hole diameter, and the hole center-to-center spacing as at least 4 times the hole diameter. For maximum bearing capacity, a larger end distance (about 4 times the diameter) is recommended.
Is an adhesive joint or a mechanical joint better?
Neither is absolutely better. An adhesive joint is more efficient and lighter for thin parts, sealed joints and spreading stress over a large area; a mechanical joint is better for thick parts, joints that must be taken apart, easy inspection and on-site installation. In pultruded structures, the bolted joint is the most common method and the hybrid joint the most reliable.
What bolts are suitable for joining composite profiles?
In corrosive environments, 316 stainless steel bolts, nuts and washers are the first choice, and 304 stainless steel can be used in milder environments. For electrically insulating applications, composite (FRP) or polymer bolts and nuts are used. Always use a wide flat washer under the bolt head and under the nut.
Why should bolts in composite parts not be over-tightened?
Composites have lower through-thickness compressive strength than metal. Excessive torque causes surface crushing, resin cracking and delamination around the hole, especially in hollow sections such as box sections and tubes. Bolts should be tightened to the manufacturer's recommended torque with a wide washer or sleeve.
Summary
Thermoset composite parts are joined by three main methods: mechanical joints (bolts and nuts, rivets, pins and self-tapping screws), adhesive joints (lap, stepped and scarf) and hybrid joints. In a mechanical joint, drilling quality, hole-to-edge distance (at least 2.5 times the diameter), hole spacing (at least 4 times the diameter), two wide flat washers, sleeves in hollow sections, 316 stainless steel bolts and limited torque are decisive, and joint capacity is usually limited by bearing in the composite, not by the bolt itself. Adhesive joints are light and efficient for thin parts but need careful surface preparation and quality control; hybrid joints combine the benefits of both with safer failure behavior. Following these principles, Nabak profiles and composite products form integrated, durable structures with no need for welding.
This article was prepared by the technical team of Nabak Composite, a manufacturer of grating, pultruded profiles, sheets and composite products.